Product Introduction ABS CHIMEI Taiwan PA‑777D is a heat‑resistant‑grade ABS resin with super heat resistance and medium impact strength, mainly processed by injection molding. It is suitable for electronic‑electrical parts, automotive components and home‑appliance products requiring heat resistance.

Main Applications

Benefiting from its ultra‑high heat resistance and good comprehensive properties, PA‑777D is widely used in the following fields:

Electronic‑Electrical Housings: Housings for televisions, copiers, monitors and other equipment.

Home‑Appliance Products: Especially for housings of heat‑generating home appliances, such as hair dryers, iron shells, space heaters.

Automotive Parts: Automotive instrument panels, radiator grilles, interior trims.

Physical Properties

Property Category Test Item Test Condition / Standard Typical Value / Range Unit
Physical Properties Density ASTM D792 1.06 g/cm³
  Melt Flow Rate (MFR) 220°C/10.0 kg, ASTM D1238 5.5‑6.0 g/10min
  Molding Shrinkage 0.3‑0.6 %
  Rockwell Hardness R‑Scale, ASTM D785 R115 R‑scale

Mechanical Properties

Property Category Test Item Test Condition / Standard Typical Value / Range Unit
Mechanical Properties Tensile Strength (Yield) ASTM D638 44.0 MPa
  Tensile Strength (Break) ISO 527‑2/50 33.0 MPa
  Elongation at Break ASTM D638 15 %
  Flexural Strength ASTM D790 66.5‑75.0 MPa
  Flexural Modulus ASTM D790 2210‑2500 MPa
  Izod Notched Impact Strength 1/8",23°C, ASTM D256 17 kg·cm/cm
  Izod Notched Impact Strength 1/4",23°C, ASTM D256 14 kg·cm/cm
  Charpy Notched Impact Strength 23°C, ISO 179 14 kJ/m²

Thermal & Flame‑Retardant Properties

Property Category Test Item Test Condition / Standard Typical Value / Range Unit
Thermal & Flame‑Retardant Properties Heat‑Distortion Temperature (HDT) 1.8 MPa, Unannealed, ASTM D648 105‑106 °C
  Heat‑Distortion Temperature (HDT) 1.8 MPa, Annealed, ASTM D648 115‑117 °C
  Vicat Softening Temperature ASTM D1525 125 °C
  Flammability Rating UL94,1.5 mm HB

Injection‑Molding Parameters

Processing Parameter Suggested Value / Range Unit
Drying Temperature 90‑105 °C
Drying Time 2‑4 (3 recommended) h
Barrel‑Rear Temperature 220‑240 °C
Barrel‑Middle Temperature 230‑250 °C
Barrel‑Front Temperature 230‑250 °C
Nozzle Temperature 220‑250 °C
Mold Temperature 30‑70 °C
Injection Pressure 50‑70 (approx.4.9‑6.86) kg/cm² or MPa
Holding Pressure 40‑60 (approx.3.92‑5.88) kg/cm² or MPa
Back Pressure 5‑15 (approx.0.49‑1.47) kg/cm² or MPa
Screw Speed 30‑100 rpm