ABS Dagu Chemical DG‑FR11 (Tianjin)

ABS Dagu Chemical DG‑FR11 (Tianjin)

Product Introduction ABS Dagu Chemical DG‑FR11 is a flame‑retardant ABS resin with UL94 V‑0 rating, designed for applications requiring flame‑retardant performance.

Main Applications

Electronics & Electrical: Router / switch housings, power adapters, smart home control modules.

Automotive Interior: Instrument panel buttons, air‑conditioner outlet grilles (compliance with automotive volatile‑organic‑compound standards required).

Industrial Components: Electric‑control box covers, safety protective shields.

Performance Parameters

Property Category Test Standard Unit Typical Value Property Description
Basic Physical Properties        
Density ISO 1183 g/cm³ 1.18‑1.22 Contains flame retardant, slightly higher than general‑purpose ABS
Melt Flow Rate (MFR) ISO 1133 g/10min 10‑15 (220°C,10kg) Medium flowability, suitable for thin‑wall injection‑molded parts
Mechanical Properties        
Tensile Strength ISO 527 MPa 45‑50 High rigidity, retains basic strength of ABS
Elongation at Break ISO 527 % 5‑10 Flame retardant reduces ductility
Flexural Strength ISO 178 MPa 70‑80 Excellent bending resistance
Flexural Modulus ISO 178 MPa 2500‑2800 High rigidity for structural support
Izod Notched Impact Strength ISO 180 kJ/m² 12‑18 (23°C) Good impact resistance, meets housing‑protection requirements
Thermal Properties        
Heat‑Deflection Temperature (HDT) ISO 75 °C 85‑90 (1.82 MPa) Suitable for long‑term service below 80°C
Vicat Softening Temperature ISO 306 °C 100‑105 Good short‑term heat resistance
Flame‑Retardant Properties        
UL94 Rating UL94 V‑0 (1.5 mm) Core advantage, certified at 1.5 mm thickness
Glow‑Wire Flammability Index (GWFI) IEC 60695 °C 850‑900 High‑grade flame‑retardant safety performance
Electrical Properties        
Dielectric Strength IEC 60243 kV/mm 25‑30 Reliable insulation performance
Volume Resistivity IEC 60093 Ω·cm >1×10¹⁵ High resistivity, suitable for electronic housings

Injection‑Molding Parameters

Process Parameter Reference Range Remarks & Instructions
Drying Treatment 80°C, 2‑4 hours Keep hopper heated to prevent re‑moisture absorption; ensure moisture content below 0.1%.
Barrel Temperature Rear zone:180‑200℃
Middle zone:190‑210℃
Front zone:200‑220℃
Nozzle:200‑230℃ (do not exceed 240°C to avoid material degradation)
Mold Temperature 40‑80℃ (commonly 50‑60℃) Higher mold temperature improves surface gloss and reduces internal stress.
Injection Pressure Adjust according to flow length and part structure May be properly reduced for high‑flow grades.
Holding Pressure Approx. 30%‑60% of injection pressure Optimize per wall thickness and structure to reduce internal stress and shrinkage.
Injection Speed Medium or medium‑high speed High‑speed improves gloss yet may cause flow marks; adopt slow‑to‑fast profile for high‑appearance requirements.
Screw Speed Proper speed for uniform plasticization (e.g. 50‑80 rpm)
Back Pressure 0.5‑1.0 MPa Facilitates uniform plasticization and degassing.

Note: All data above is for reference only.