AS Chi Mei Taiwan PN‑107L125

AS Chi Mei Taiwan PN‑107L125

Product Introduction AS Chi Mei Taiwan PN‑107L125 resin is a high‑flow, high‑transparency acrylonitrile‑styrene copolymer (AS/SAN). It combines good rigidity and excellent processability, and complies with relevant food‑contact regulatory certifications.

Main Applications

Food Packaging & Containers: Food containers, sealing cans, tableware and kitchen appliances. High transparency plus compliance with EU 10/2011 and Chinese GB4806 standards make it ideal for these scenarios.

Daily‑use Consumer Goods & Cosmetic Packaging: Cosmetic cases & cosmetic packaging, toothbrush handles, pen barrels, refrigerator fruit‑vegetable boxes and TV bases.

Electronic & Electrical Components: Electrical sockets, housings, instrument casings, battery boxes, storage‑battery enclosures and junction boxes. Reliable electrical insulation and mechanical strength meet component performance requirements.

Automotive Industry: Automotive parts including head‑lamp housings, rear‑view mirror housings and instrument panels.

Industrial & Other Articles: Oil‑resistant mechanical parts, tractor fuel tanks, packaging containers and stationery.

Performance Parameters

Property Category Test Item Typical Value Test Condition / Standard
Physical Properties Density 1.06 g/cm³ ISO 1183, 23℃
  Melt Volume Rate (MVR) 44 ml/10min or 58.0 cm³/10min 220°C /10 kg, ISO 1133
  Molding Shrinkage 0.2‑0.7 % ISO 294‑4
Mechanical Properties Tensile Strength (Yield) 52 MPa or 65.0 MPa ISO 527
  Flexural Strength 178 MPa or 89.0 MPa ISO 178
  Flexural Modulus 2600 MPa or 2.6 GPa ISO 178
  Izod Notched Impact Strength 2.0 kJ/m² ISO 180/1A or ISO 179
  Rockwell Hardness (M‑Scale) M‑80 or 155 N/mm² (ball indentation) ASTM D785 or ISO 2039‑1
  Elongation at Break 4.0 % ISO 527
Thermal Properties Heat‑Deflection Temperature (HDT) 88.0 °C (un‑annealed); 99.0 °C (annealed) ISO 75‑2/A, 1.8 MPa
  Vicat Softening Temperature 101‑108 °C (varies by test condition) ISO 306
Other Properties Flammability (UL 94) HB (1.5 mm) UL 94
  Food‑contact Compliance Compliant with EU 10/2011 & China GB4806

Injection‑Molding Parameters

Process Parameter Reference Range Remarks & Instructions
Drying Treatment 75‑80°C, 3‑4 hours AS resin is hygroscopic. Sufficient drying is required (moisture content below 0.1% recommended), otherwise silver streaks and bubbles may occur on finished‑part surfaces.
Barrel Temperature Feed zone:160‑180℃ | Compression zone:180‑200℃ | Nozzle:180‑210℃ Use lower melt temperature for thick‑wall products. Prevent material degradation; avoid long‑term residence of molten material inside high‑temperature barrel.
Mold Temperature 40‑60℃ For high‑precision molded parts within this range. Mold temperature directly affects appearance, shrinkage and warpage of finished products.
Injection Pressure 50‑70 kg/cm² Adjust according to flow length and product structure.
Holding Pressure 40‑60 kg/cm² Approx.30%‑60% of injection pressure. Optimize according to wall thickness and product structure to reduce internal stress and shrinkage.
Back Pressure 5‑15 kg/cm² Proper back‑pressure ensures uniform plasticization and degassing.
Injection Speed High‑speed injection recommended Beneficial for good surface gloss, color performance and minimizing weld‑lines.

Note: All data above is for reference only.