PA1010 Shanghai Celluloid 09‑12

PA1010 Shanghai Celluloid 09‑12 Resin

Material Introduction: PA1010 Shanghai Celluloid 09‑12 is a high‑impact‑performance engineering plastic. It features favorable mechanical properties, excellent chemical‑resistance, good electrical performance and heat‑resistance. It is highly suitable for mechanical parts, chemical and electrical components requiring high‑impact and high‑strength performance.

Main Applications

Precision‑mechanical components & wear‑resistant transmission parts (core application): Gears, bearings, shaft sleeves, bushings, pulleys, sprockets, cams, valve seals, valve seats.

Automotive & construction‑machinery hydraulic and fuel‑system components: High‑pressure oil hoses (critical application), pipe joints, quick‑connect couplings, sealing rings, gaskets, filter‑element parts, fuel‑tank components.

Electrical‑electronic components & cable sheaths: Connectors, terminals, coil bobbins, cable ties, fasteners, electrical housings, supports, optical‑cable jackets.

Textile‑machinery dedicated wear‑resistant accessories: Shuttles, yarn guides, picking sticks, gears, cams, bearings.

Other industrial & special applications: Food‑processing & packaging‑machine parts, medical‑device components, sports‑equipment parts, precision injection‑molded articles.

Performance Parameters

Performance Category Test Item Test Standard Typical Value Unit Remarks & Interpretation
Physical Properties Density GB 1033 1.04 g/cm³ High‑impact PA1010 grade
  Viscosity Number 80‑99
Mechanical Properties Tensile Strength GB 1040 45 MPa
  Flexural Strength GB 1042 75 MPa
  Notched Charpy Impact Strength GB 1043 17 kJ/m² High‑impact characteristic
  Flexural Modulus 1500 MPa
Thermal Properties Heat‑Distortion Temperature (HDT) GB 1634 40 °C
  UL94 Rating UL 94 HB Non‑flame‑retardant grade
Electrical Properties Volume Resistivity GB 1410 10¹² Ω·cm Good insulation performance
  Dielectric Constant GB 1409 3.5
  Dielectric Loss Factor 0.02

Processing Parameters

Processing Item Recommended Range / Operating Points Notes & Explanations
Pre‑drying Mandatory drying. Hot‑air drying:90℃±5℃ for 4‑5 h;Vacuum drying:85℃±5℃. Prevent bubbles and silver streaks on finished parts, avoid high‑temperature hydrolysis of material.
Barrel Temperature Rear zone:190‑210℃;Middle zone:200‑220℃;Front zone:210‑230℃ Narrow melt‑temperature window, precise control required. Excessively high temperature or long residence time will cause thermal‑oxidative degradation.
Nozzle Temperature 200‑210℃
Mold Temperature 20‑40℃
Injection Pressure 60‑80 MPa
Extrusion Temperature Barrel zones:250℃,260℃,270℃,280℃;Die‑head temperature:200‑210℃

Disclaimer: All above data is for reference only.