PPA DuPont HTNFR52G30BL
PPA DuPont HTNFR52G30BL Resin
Material Introduction: PPA DuPont HTNFR52G30BL is a high‑performance polyphthalamide material. It features good high‑temperature resistance, high strength & rigidity, low moisture absorption, excellent dimensional stability and chemical resistance.
Main Applications
Electrical & electronic connectors, automotive components (especially under‑hood parts), power‑tool accessories.
Performance Parameters
| Performance Category | Test Item | Test Condition / Standard | Typical Value | Unit | Remarks & Interpretation |
|---|---|---|---|---|---|
| Physical Properties | Density | ISO 1183 | 1.62 | g/cm³ | Reinforced flame‑retardant PPA |
| Molding Shrinkage (flow direction) | ISO 294‑4 | 0.30 | % | ‑ | |
| Molding Shrinkage (cross‑flow direction) | ISO 294‑4 | 0.80 | % | ‑ | |
| Mechanical Properties | Tensile Strength at Break | ISO 527‑2 / ASTM D638 | 160‑172 | MPa | ‑ |
| Tensile Modulus | ISO 527‑2 | 11800 | MPa | ‑ | |
| Flexural Strength | ISO 178 | 240 | MPa | ‑ | |
| Flexural Modulus | ISO 178 / ASTM D790 | 10000‑11400 | MPa | ‑ | |
| Charpy Notched Impact Strength (23°C) | ISO 179/1eA | 10 | kJ/m² | ‑ | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 1.8 MPa, unannealed, ISO 75‑2/A | 282‑285 | ℃ | ‑ |
| Melting Temperature | ISO 11357‑3 | 310 | ℃ | ‑ | |
| Glass Transition Temperature | ISO 11357‑2 | ca.90 | ℃ | ‑ | |
| Electrical Properties | Comparative Tracking Index(CTI) | IEC 60112 | 525‑600 | V | ‑ |
| Volume Resistivity | IEC 60093 | >1.0E+15 | Ω·cm | ‑ | |
| Flammability | UL94 Rating | UL 94 | V‑0 (0.75 mm) | ‑ | ‑ |
Processing Parameters
| Processing Item | Recommended Range / Operation Key Points | Remarks & Instructions |
|---|---|---|
| Pre‑drying | Drying is mandatory. Dry at 100‑120 ℃ for 4‑6 hours. | Moisture content shall be kept below 0.05% to prevent molecular weight reduction caused by hydrolysis, silver streaks, bubbles and other defects. |
| Barrel Temperature | Melt temperature range:310‑330 ℃ | Critical processing window. Low temperature leads to poor flowability; excessive temperature causes material degradation. Residence time inside barrel shall not exceed 10 minutes. |
| Mold Temperature | 120‑140 ℃, minimum 90 ℃ is recommended. | Higher mold temperature reduces internal stress, improves surface gloss and dimensional stability, and ensures sufficient crystallization. |
| Injection Pressure | Adjust according to product structure and wall thickness; medium‑high pressure is recommended. | Ensure complete mold filling. |
| Injection Speed | Medium speed. | Excessive speed may cause jet marks; insufficient speed may lead to short shots. |
| Screw Speed | Medium speed. | Avoid excessive shear force which may break glass fibers or degrade the material. |
Disclaimer: All above data is for reference only.