PPA DuPont HTN51G35HSL

PPA DuPont HTN51G35HSL Resin

Material Introduction: PPA DuPont HTN51G35HSL is a high‑performance polyphthalamide material. It delivers outstanding heat resistance, high strength & high rigidity, low moisture absorption, excellent mechanical strength and dimensional stability for demanding engineering applications.

Main Applications

Automotive field: Components for engine system and fuel system, such as sensor housings and fuel‑line parts.

Electrical & electronics: Key electronic components including connectors and controllers.

Industrial parts: Bearing seats, pulleys and other structural components.

Performance Parameters

Performance Category Test Item Test Condition / Standard Typical Value Unit Remarks & Interpretation
Physical Properties Density ISO 1183 1.47 g/cm³ Glass‑fiber reinforced PPA
  Molding Shrinkage (flow direction) ISO 294‑4 0.20‑0.30 %
  Molding Shrinkage (cross‑flow direction) ISO 294‑4 0.60‑0.90 %
Mechanical Properties Tensile Strength at Break ISO 527‑2 215‑220 MPa
  Tensile Modulus ISO 527‑2 12000‑12500 MPa
  Flexural Modulus ISO 178 / ASTM D790 10300‑10500 MPa
  Charpy Notched Impact Strength (23°C) ISO 179/1eA 11 kJ/m²
  Charpy Unnotched Impact Strength (23°C) ISO 179/1eU 65‑70 kJ/m²
Thermal Properties Heat‑Distortion Temperature(HDT) 1.8 MPa, ISO 75‑2/A 264
  Heat‑Distortion Temperature(HDT) 0.45 MPa, ISO 75‑2/B 276‑284
  Melting Temperature ISO 11357‑3 300
  Glass Transition Temperature ISO 11357‑3 141
  Coefficient of Linear Thermal Expansion (flow direction) ISO 11359‑2 1.8E‑5 cm/cm/℃
  Coefficient of Linear Thermal Expansion (cross‑flow direction) ISO 11359‑2 5.5E‑5‑5.8E‑5 cm/cm/℃
Electrical Properties Volume Resistivity IEC 60093 1.0E+15 Ω·cm
  Dielectric Strength IEC 60243‑1 / ASTM D149 27.1‑36 kV/mm
  Comparative Tracking Index(CTI) IEC 60112 600 V
Flammability UL94 Rating 0.75 mm, UL 94 HB

Processing Parameters

Processing Item Recommended Range / Operation Key Points Remarks & Instructions
Pre‑drying Drying is mandatory. Dry at 120‑140 ℃ for 4‑6 hours. Moisture content shall be kept below 0.1% to prevent molecular weight reduction caused by hydrolysis, silver streaks, bubbles and other defects.
Barrel Temperature Melt temperature range:290‑330 ℃(approx.615‑650°F) Critical processing window. Low temperature leads to poor flowability; excessive temperature causes material degradation. Residence time inside barrel shall not exceed 10 minutes.
Mold Temperature 90‑130 ℃, minimum 90 ℃, up to 135 ℃(approx.275°F) per reference data. Higher mold temperature reduces internal stress, improves surface gloss and dimensional stability, and ensures sufficient crystallization.
Injection Pressure Adjust according to product structure and wall thickness.
Injection Speed Medium speed.
Screw Speed Medium speed. Avoid excessive shear force which may break glass fibers or degrade the material.

Disclaimer: All above data is for reference only.