PP Ningbo Jinfa T30S
PP Ningbo Jinfa T30S Resin
Material Introduction: PP Ningbo Jinfa T30S is widely‑used low‑MFR drawing‑grade homopolymer polypropylene, also frequently used for injection molding.
Main Applications
Food packaging: Non‑toxic, tasteless and odor‑free, complying with food‑contact standards including GB 9693‑88 and US FDA. Suitable for food containers, pharmaceutical packaging and other direct‑food‑contact applications.
Woven products: Traditional and primary application, including woven bags, tarpaulins, FIBC bulk bags, carpet backing, artificial turf, strapping ropes and packaging ropes. Good tensile strength and low elongation satisfy these working conditions.
Injection‑molded products: Daily‑use articles and general‑purpose components such as buckets, basins, stools, toys and household goods. Good flow property adapts to injection‑molding processing.
Films & fibers: Applied for tear‑film, monofilaments and spinning fibers.
Performance Parameters
| Performance Category | Test Item | Typical Value | Test Condition / Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|
| Physical Properties | Density | 0.90‑0.91 g/cm³ | Typical PP value | Low‑MFR drawing‑grade homopolymer PP |
| Melt Flow Rate(MFR) | 2.0‑4.0 g/10min | 230℃/2.16kg, GB/T 3682 | ‑ | |
| Isotactic Index | ≥96.0 % | GB/T 2412 | ‑ | |
| Mechanical Properties | Tensile Yield Strength | 28‑35 MPa | GB/T 1040 | ‑ |
| Flexural Modulus | 1280‑1550 MPa | GB/T 9341 | ‑ | |
| Izod Notched Impact Strength | ~55 J/m (23℃) | ‑ | ‑ | |
| Rockwell Hardness(R scale) | 90‑105 R | GB/T 9342 | ‑ | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | ≥86 ℃ (0.45 MPa) | GB/T 1634 | ‑ |
| Vicat Softening Temperature | ≥150 ℃ | GB/T 1633 | ‑ | |
| Other Properties | Ash Content | ≤0.04 % | GB/T 9345 | ‑ |
Processing Parameters
| Processing Item | Reference Range | Remarks & Instructions |
|---|---|---|
| Drying Treatment | Normally not required | PP water absorption approx.0.01%‑0.04%. Drying is unnecessary under proper storage. Dry at 80‑100 ℃ for 1‑2 h if material gets damp. |
Disclaimer: All above data is for reference only。