PP Maoming Petrochemical K7726H Resin
PP Maoming Petrochemical K7726H Resin
Material Introduction: PP Maoming Petrochemical K7726H is high‑flow impact‑resistant block‑copolymer polypropylene. It delivers good stiffness‑toughness balance, low odor, high whiteness and excellent processability for multiple application fields.
Main Applications
Home appliances: Mainly used for washing machine inner tubs, outer tubs and related components. Low‑odor property is well‑suited for home appliances with high hygiene‑safety requirements. This grade is massively adopted by Midea‑owned Toshiba home‑appliance products for export to Japan.
Automotive industry: For automotive interior & exterior parts, used as base resin for modified automotive interior components.
Thin‑wall injection‑molded articles: High melt flowability fits thin‑wall production and helps reduce raw‑material consumption.
Performance Parameters
| Performance Category | Test Item | Typical Value | Test Condition / Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|
| Physical Properties | Melt Flow Rate(MFR) | 24.2‑35.0 g/10min | 230℃/2.16kg, GB/T 3682 | High‑flow block‑copolymer PP |
| Ash Content | ≤0.02 % | GB/T 9345.1 | ‑ | |
| Mechanical Properties | Tensile Yield Strength | 25.5‑29.1 MPa | GB/T 1040.2 | ‑ |
| Flexural Modulus | 1090‑1310 MPa | GB/T 9341 | ‑ | |
| Izod Notched Impact Strength | 12 kJ/m² (23℃);4.7 kJ/m² (-20℃) | GB/T 1843 | ‑ | |
| Rockwell Hardness | R‑100 | GB/T 9342 | ‑ | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 95‑100 ℃ | GB/T 1634.2 (1.82 MPa) | ‑ |
| Other Properties | Yellow Index | ≤4 △Y.I. | ‑ | ‑ |
Processing Parameters
| Processing Item | Reference Range | Remarks & Instructions |
|---|---|---|
| Drying Treatment | Normally not required | PP features extremely low water‑absorption. Drying is unnecessary under proper storage. Dry at 80 ℃ for 1‑2 h if material gets damp. |
| Barrel Temperature | 200‑275℃ | Homopolymer PP melting point:164‑170℃. Do not exceed 275 ℃ to prevent material degradation. |
| Mold Temperature | 40‑80℃ | Recommended:50℃. Higher mold temperature improves surface gloss, dimensional stability and weld‑line strength; lower mold temperature shortens molding cycle. |
| Injection Pressure | 68.6‑137.2 MPa, up to 1800 bar | Adjust per flow‑length and part structure. Appropriately lower injection pressure for this high‑flow grade. |
| Injection Speed | High‑speed injection | High‑speed injection minimizes internal pressure. Try low‑speed injection at higher melt temperature if surface defects occur. |
| Holding Pressure | 30%‑60% of injection pressure | Sufficient holding pressure reduces shrinkage and sink marks. Avoid excessive holding time to prevent high internal stress. |
| Back Pressure | 0.5‑1.0 MPa | Moderate back‑pressure improves melt homogenization and venting. Not mandatory; too low back‑pressure may cause air entrapment in melt. |
| Screw Speed | 50‑100 rpm | Avoid excessive screw speed to prevent shear‑induced overheating. |
Disclaimer: All above data is for reference only.