PP Formosa Plastics Taiwan 3080 Resin
PP Formosa Plastics Taiwan 3080 Resin
Material Introduction: PP Formosa Plastics Taiwan 3080 is impact‑copolymer polypropylene. It features medium‑impact resistance, good rigidity and balanced mechanical properties, and complies with food‑contact regulations.
Main Applications
Automotive parts: automobile bumpers, interior panels, motorcycle accessories.
Home‑appliance housings: TV housings, computer cases, electrical‑equipment housings.
Daily‑use products: furniture, toys, office supplies, battery housings.
Food‑contact applications: compliant with FDA 21 CFR 177.1520 for food‑related applications.
Performance Parameters
| Performance Category | Test Item | Test Condition | Value / Range | Unit | Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|---|---|
| Basic Properties | Melt Flow Rate(MFR) | 230℃/2.16kg | 8.0‑9.0 | g/10 min | ASTM D1238, ISO 1133 | Copolymer PP flow index. |
| Density | ‑ | 0.90 | g/cm³ | ASTM D792, ISO 1183 | ‑ | |
| Mechanical Properties | Tensile Yield Strength | ‑ | 27.5‑29.0 | MPa | ISO 527‑2, ISO 527 | ‑ |
| Elongation at Break | ‑ | 200‑500 | % | ISO 527‑2, ISO 527 | High ductility. | |
| Flexural Modulus | ‑ | 981‑1422 | MPa | ISO 178 | Stiffness range. | |
| Izod Notched Impact Strength | 23℃ | 98 J/m / 10 kg·cm/cm | J/m or kg·cm/cm | ISO 180, ASTM D256 | Room‑temperature impact. | |
| Izod Notched Impact Strength | -20℃ | 44 J/m / 4.5 kg·cm/cm | J/m or kg·cm/cm | ISO 180, ASTM D256 | Low‑temperature impact. | |
| Rockwell Hardness | R‑scale | 100‑105 | ‑ | ASTM D785, ISO 2039‑2 | Surface hardness. | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 1.8 MPa, non‑annealed | 105‑130 | ℃ | ISO 75‑2/A, ASTM D648 | High‑load heat resistance. |
| Vicat Softening Temperature | ‑ | 140‑155 | ℃ | ISO 306, ASTM D1525 | Heat‑resistance indicator. | |
| Other Properties | Molding Shrinkage | ‑ | 1.0‑1.7 | % | Internal / FPC Method | Mold‑design reference. |
| UL Flame Retardant Rating | ‑ | HB | ‑ | UL 94 | Flammability grade. |
Injection‑Molding Process Parameters
| Process Item | Suggested Range / Description | Remarks |
|---|---|---|
| Drying treatment | Generally unnecessary; dry at 80℃ for 1‑2 h if damp under poor storage condition | PP low‑moisture‑absorption feature. |
| Barrel rear zone(feed section) | 160‑200℃ | Prevent thermal degradation. |
| Barrel middle zone(compression section) | 180‑220℃ | ‑ |
| Barrel front zone(metering section) | 200‑240℃ | ‑ |
| Nozzle temperature | 200‑240℃ | ‑ |
| Melt temperature | ‑ | 220‑280℃ |
| Mold temperature | 20‑70℃, recommended 40‑60℃ | Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage. |
| Injection pressure | 80‑140 MPa(800‑1400 bar) | Higher pressure for thin‑wall or complex‑structure parts. |
| Holding pressure | 30%‑60% of injection pressure | Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time. |
| Back pressure | 5‑20 MPa(50‑200 bar) | ‑ |
| Injection speed | Medium speed; high‑speed injection required for thin‑wall packaging containers. | ‑ |
| Screw speed | High screw speed(linear velocity 1.3 m/s) is permitted | Complete plasticization before cooling phase finishes. |
| Runner & Gate | Pin‑point gate or multi‑point gate; hot‑runner system(heated / insulated type). Gate shall be set at thick‑wall position of product, otherwise shrinkage defect easily occurs. | Mold‑design suggestion. |
Disclaimer: All above data is for reference only.