PP CNOOC Shell EP548R Resin
PP CNOOC Shell EP548R Resin
Material Introduction: PP CNOOC Shell EP548R is medium‑impact copolymer polypropylene. It features good rigidity, balanced mechanical properties and antistatic property, widely used in various injection‑molding fields.
Main Applications
Automotive accessories: automotive components.
Home appliance manufacturing: washing‑machine parts, household‑appliance products, power‑tool housings.
Household articles: furniture, daily goods, toys, thin‑wall parts, sports goods, food‑contact containers (food‑contact compliance mentioned for this grade).
Daily‑chemical packaging.
Performance Parameters
| Performance Category | Test Item | Test Condition | Reference Value | Unit | Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|---|---|
| Basic Properties | Melt Flow Rate(MFR) | 230℃/2.16kg | 21‑28 | g/10 min | ISO 1133, ASTM D1238 | High‑flow copolymer PP. |
| Density | ‑ | 0.90‑0.905 | g/cm³ | ISO 1183, ASTM D1505 | Typical copolymer PP density. | |
| Mechanical Properties | Tensile Yield Strength | ‑ | 25‑27 | MPa | ISO 527, ASTM D638 | ‑ |
| Flexural Modulus | ‑ | 1250‑1550 | MPa | ISO 178, ASTM D790 | Rigidity range. | |
| Elongation at Break | ‑ | >50 | % | ISO 527, ASTM D638 | ‑ | |
| Charpy Notched Impact Strength | 23℃ | 6‑14 | kJ/m² | ISO 179, ASTM D256 | Room‑temperature notched impact. | |
| Charpy Un‑notched Impact Strength | 23℃ | No Break | kJ/m² | ISO 179, ASTM D256 | Un‑notched non‑break performance. | |
| Rockwell Hardness | R‑scale | 86 | ‑ | ASTM D785 | Surface hardness. | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 0.45MPa, non‑annealed | 95‑107 | ℃ | ISO 75, ASTM D648 | Low‑load heat‑resistance range. |
| Vicat Softening Temperature | B50 (50℃/h,50N) | 149 | ℃ | ISO 306, ASTM D1525 | Heat‑resistance index. | |
| Other Features | Antistatic | ‑ | Yes | ‑ | ‑ | Antistatic modification grade. |
| Nucleated | ‑ | Yes | ‑ | ‑ | Nucleation modified. |
Injection‑Molding Process Parameters
| Process Item | Suggested Range / Description | Remarks |
|---|---|---|
| Drying treatment | Generally unnecessary; dry at 80℃ for 1‑2 h if damp under poor storage condition | PP low‑moisture‑absorption feature. |
| Barrel rear zone(feed section) | 160‑200℃ | Prevent thermal degradation. |
| Barrel middle zone(compression section) | 180‑220℃ | ‑ |
| Barrel front zone(metering section) | 200‑240℃ | ‑ |
| Nozzle temperature | 200‑240℃ | ‑ |
| Mold temperature | 40‑80℃, recommended 50℃ | Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage. |
| Injection pressure | 80‑140 MPa(800‑1400 bar) | Higher pressure for thin‑wall or complex‑structure parts. |
| Holding pressure | 30%‑60% of injection pressure | Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time. |
| Injection speed | Medium speed; high‑speed injection required for thin‑wall packaging containers. | ‑ |
| Screw speed | High screw speed(linear velocity 1.3 m/s) is permitted | Complete plasticization before cooling phase finishes. |