PP Zhejiang Petrochemical K8003 Resin
PP Zhejiang Petrochemical K8003 Resin
Material Introduction: PP Zhejiang Petrochemical K8003 is block‑copolymer polypropylene. It possesses excellent mechanical properties, heat resistance and favorable processing stability.
Main Applications
Automotive parts: manufacturing of automotive components.
Home appliances: TV housings, radio housings, electrical insulating materials.
Industrial parts: anti‑corrosion pipes, sheets, storage tanks.
Packaging materials: flat yarn, fiber, packaging films.
Performance Parameters
| Performance Category | Test Item | Test Condition | Reference Value | Unit | Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|---|---|
| Basic Properties | Melt Flow Rate(MFR) | 230℃/2.16kg | 2.0‑3.0 | g/10 min | GB/T 3682.1 | Low‑flow block‑copolymer PP. |
| Mechanical Properties | Tensile Yield Strength | ‑ | ≥22‑≥26 | MPa | GB/T 1040.2 | Strength range. |
| Flexural Modulus | ‑ | ≥1000‑≥1300 | MPa | GB/T 9341 | Rigidity range. | |
| Charpy Notched Impact Strength | 23℃ | To be confirmed | kJ/m² | GB/T 1043 | ‑ | |
| Izod Impact Strength | -20℃ | ≥5.0‑≥7.0 | kJ/m² | ‑ | Low‑temperature impact index. | |
| Elongation at Break | ‑ | To be confirmed | % | ‑ | ‑ | |
| Rockwell Hardness | R‑scale | To be confirmed | R | ‑ | ‑ | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 0.46MPa, non‑annealed | ≥80‑≥93 | ℃ | ‑ | Low‑load heat‑resistance range. |
| Other Properties | Cleanliness(impurity) | ‑ | ≤20‑≤60 | grains/kg resin | ‑ | Impurity particle index. |
| Cleanliness(colored particle) | ‑ | ≤5‑≤20 | grains/kg resin | ‑ | Colored‑particle control index. |
Injection‑Molding Process Parameters
| Process Item | Suggested Range / Description | Remarks |
|---|---|---|
| Drying treatment | Generally unnecessary; dry at 80℃ for 1‑2 h under poor storage condition | PP low‑moisture‑absorption feature. |
| Barrel rear zone(feed section) | 160‑200℃ | Prevent thermal degradation. |
| Barrel middle zone(compression section) | 180‑220℃ | ‑ |
| Barrel front zone(metering section) | 200‑240℃ | ‑ |
| Nozzle temperature | 200‑240℃ | ‑ |
| Mold temperature | 40‑80℃, recommended 50℃ | Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage. |
| Injection pressure | 80‑140 MPa(800‑1400 bar) | Higher pressure for thin‑wall or complex‑structure parts. |
| Holding pressure | 30%‑60% of injection pressure | Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time. |
| Injection speed | Medium speed; high‑speed injection required for thin‑wall packaging containers. | ‑ |
| Screw speed | High screw speed(linear velocity 1.3 m/s) is permitted | Complete plasticization before cooling phase finishes. |
Disclaimer: All above data is for reference only.