PP Dushanzi Petrochemical K8003 Resin

PP Dushanzi Petrochemical K8003 Resin

Material Introduction: PP Dushanzi Petrochemical K8003 is injection‑molding block‑copolymer polypropylene. It delivers high‑impact resistance and favorable mechanical properties, widely used for industrial components.

Main Applications

Automotive parts: automotive components.

Heavy‑load parts: load‑bearing industrial components.

Daily‑use articles: baby strollers.

Other applications: home‑appliance parts, thin‑wall products.

Performance Parameters

Performance Category Test Item Test Condition Reference Value Unit Reference Standard Remarks & Interpretation
Basic Properties Melt Flow Rate(MFR) 230℃/2.16kg 2.5 g/10 min ASTM D‑1238 Low‑flow block‑copolymer PP.
  Density 0.90 g/cm³ ASTM D‑1505 Typical copolymer PP density.
Mechanical Properties Tensile Yield Strength 26 MPa ASTM D‑638
  Flexural Modulus 1300 MPa ASTM D‑790A Rigidity performance.
  Elongation at Break >200 % ASTM D‑638 High ductility.
  Izod Impact Strength V‑notch,23℃ 70 J/m ASTM D‑256 Room‑temperature impact resistance.
  Rockwell Hardness 75 R scale ASTM D‑785 Surface hardness.
Thermal Properties Heat‑Distortion Temperature(HDT) 0.46MPa, non‑annealed 93 ASTM D‑648 Low‑load heat resistance.
Other Properties Yellow Index 4 ASTM E313‑00 Color‑stability reference.

Injection‑Molding Process Parameters

Process Item Suggested Range / Description Remarks
Drying treatment Generally unnecessary; dry at 80℃ for 1‑2 h under poor storage condition PP low‑moisture‑absorption feature.
Barrel rear zone(feed section) 160‑200℃ Prevent thermal degradation.
Barrel middle zone(compression section) 180‑220℃
Barrel front zone(metering section) 200‑240℃
Nozzle temperature 200‑240℃
Mold temperature 40‑80℃, recommended 50℃ Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage.
Injection pressure 80‑140 MPa(800‑1400 bar) Higher pressure for thin‑wall or complex‑structure parts.
Holding pressure 30%‑60% of injection pressure Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time.
Injection speed Medium speed; high‑speed injection required for thin‑wall packaging containers.
Screw speed High screw speed(linear velocity 1.3 m/s) is permitted Complete plasticization before cooling phase finishes.

Disclaimer: All above data is for reference only.