PP Orient Energy K8003 Resin

PP Orient Energy K8003 Resin

Material Introduction: PP Orient Energy K8003 is high‑impact block‑copolymer polypropylene. It delivers outstanding toughness, favorable heat resistance and dimensional stability for multiple application fields.

Main Applications

Packaging containers: turnover boxes, bottles, paint buckets, large‑size containers and heavy‑duty packaging.

Automotive parts: automotive components.

Industrial parts: load‑bearing industrial components.

Consumer goods: baby strollers, power‑tool housings, children’s carts.

Performance Parameters

Performance Category Test Item Test Condition Reference Value Unit Reference Standard Remarks & Interpretation
Basic Properties Melt Flow Rate(MFR) 230℃/2.16kg 2.5 / 12 g/10 min ASTM D1238, ISO 1133 Dual MFR reference values.
  Density 0.90 g/cm³ ASTM D792, ASTM D1505, ISO 1183 Typical copolymer PP density.
Mechanical Properties Tensile Yield Strength 25‑26 MPa ASTM D638, ISO 527
  Flexural Modulus 1000‑1300 MPa ASTM D790, ISO 178 Stiffness range.
  Elongation at Break >200 / 300 % ASTM D638, ISO 527 High ductility.
  Izod Notched Impact Strength 23℃ N.B(no‑break) / 70 J/m / 40 kJ/m² J/m or kJ/m² ASTM D256, ISO 179 Non‑break feature for high‑toughness grade.
  Rockwell Hardness R‑scale 70‑85 R scale ASTM D785, ISO 2039‑2 Surface hardness range.
Thermal Properties Heat‑Distortion Temperature(HDT) 0.45MPa/0.46MPa/4.6kg/cm², non‑annealed 90‑100 / 74 ASTM D648, ISO 75 Low‑load heat‑resistance range.
Other Properties Molding Shrinkage 1.4‑1.8 % Mold‑design reference.

Injection‑Molding Process Parameters

Process Item Suggested Range / Description Remarks
Drying treatment Generally unnecessary; dry at 80℃ for 1‑2 h if damp under poor storage condition PP low‑moisture‑absorption feature.
Barrel rear zone(feed section) 180‑200℃ Prevent thermal degradation.
Barrel middle zone(compression section) 200‑220℃
Barrel front zone(metering section) 210‑230℃
Nozzle temperature 210‑230℃
Mold temperature 40‑80℃, recommended 50‑70℃ Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage.
Injection pressure 70‑120 MPa Higher pressure for thin‑wall or complex‑structure parts.
Holding pressure 40%‑60% of injection pressure Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time.
Injection speed Medium‑low speed Medium‑low injection speed recommended for high‑impact grade, to optimize molecular orientation and reduce internal stress.
Screw speed Medium screw speed Avoid excessive shear heat leading to material degradation.

Disclaimer: All above data is for reference only.