PP Daelim EP300R Resin

PP Daelim EP300R Resin

Material Introduction: PP Daelim EP300R is high‑impact block‑copolymer polypropylene. It delivers excellent low‑temperature impact resistance, favorable rigidity and low‑warpage performance, widely applied in multiple injection‑molding fields.

Main Applications

Home appliances: washing‑machine inner drums, electrical appliances and related components.

Thin‑wall packaging: thin‑wall packaging products.

Daily‑use articles: household utensils and containers.

Electrical & electronic components: electronic and electrical parts.

Performance Parameters

Performance Category Test Item Test Condition Reference Value Unit Reference Standard Remarks & Interpretation
Basic Properties Melt Flow Rate(MFR) 230℃/2.16kg 30 g/10 min ASTM D‑1238L High‑flow injection‑molding copolymer PP.
  Density 0.9 g/cm³ ASTM D‑1505 Typical PP copolymer density.
Mechanical Properties Tensile Strength 240(≈23.5 MPa) kg/cm² or MPa ASTM D‑638 Unit conversion marked.
  Flexural Strength 10500(≈1030 MPa) kg/cm² or MPa ASTM D‑790
  Elongation at Break 5 % ASTM D‑638
  Izod Notched Impact Strength 23℃ 13 kg·cm/cm ASTM D‑256 Room‑temperature impact performance.
  Izod Notched Impact Strength -20℃ 5 kg·cm/cm ASTM D‑256 Low‑temperature impact resistance.
  Rockwell Hardness R‑scale 85 ASTM D‑785 Surface hardness.
Thermal Properties Vicat Softening Point 150 ASTM D‑1525 Heat‑resistance indicator.

Injection‑Molding Process Parameters

Process Item Suggested Range / Description Remarks
Drying treatment Generally unnecessary; dry at 80℃ for 1‑2 h under poor storage condition PP low‑moisture‑absorption feature.
Barrel rear zone(feed section) 160‑200℃ Prevent thermal degradation.
Barrel middle zone(compression section) 180‑220℃
Barrel front zone(metering section) 200‑240℃
Nozzle temperature 200‑240℃
Mold temperature 40‑80℃, recommended 50℃ Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage.
Injection pressure 80‑140 MPa(800‑1400 bar) Higher pressure for thin‑wall or complex‑structure parts.
Holding pressure 30%‑60% of injection pressure Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time.
Injection speed Medium speed; high‑speed injection required for thin‑wall packaging containers.
Screw speed High screw speed(linear velocity 1.3 m/s) is permitted Complete plasticization before cooling phase finishes.

Disclaimer: All above data is for reference only.

 