PP Orient Energy PPH‑Y26 Resin
PP Orient Energy PPH‑Y26 Resin
Material Introduction: PP Orient Energy PPH‑Y26 is fiber‑grade homopolymer polypropylene. Mainly applied for fiber products according to industry common knowledge.
Main Applications
Fiber & non‑woven fabrics: polypropylene filament, long fiber, short fiber, non‑woven fabrics for medical hygiene materials and household articles.
Home textiles: fiber products such as garments and blankets.
Other applications: injection‑molded articles including household utensils and thin‑wall products.
Performance Parameters
| Performance Category | Test Item | Test Condition | Reference Value | Unit | Reference Standard | Remarks & Interpretation |
|---|---|---|---|---|---|---|
| Basic Properties | Melt Flow Rate(MFR) | 230℃/2.16kg | 25‑26 | g/10 min | ASTM D1238, ISO 1133 | High‑flow fiber‑spinning homopolymer PP. |
| Density | ‑ | 0.90‑0.91 | g/cm³ | ASTM D792, ISO 1183 | Typical PP density range. | |
| Mechanical Properties | Tensile Yield Strength | ‑ | ≥34.5 | MPa | ASTM D638, ISO 527 | High tensile strength for fiber spinning. |
| Flexural Modulus | ‑ | ≥1470 | MPa | ASTM D790, ISO 178 | High‑rigidity grade. | |
| Elongation at Break | ‑ | >200 | % | ASTM D638, ISO 527 | Good ductility. | |
| Thermal Properties | Heat‑Distortion Temperature(HDT) | 0.45 MPa, non‑annealed | ≥100 | ℃ | ASTM D648, ISO 75 | Heat‑resistance reference. |
| Other Properties | Isotactic Index | ‑ | ≥96 | % | ‑ | High isotacticity for fiber processing. |
Injection‑Molding Process Parameters
| Process Item | Suggested Range / Description | Remarks |
|---|---|---|
| Drying treatment | Generally unnecessary; dry at 80℃ for 1‑2 h if damp under poor storage condition | PP low‑moisture‑absorption feature. |
| Barrel rear zone(feed section) | 160‑200℃ | Prevent thermal degradation. |
| Barrel middle zone(compression section) | 180‑220℃ | ‑ |
| Barrel front zone(metering section) | 200‑240℃ | ‑ |
| Nozzle temperature | 200‑240℃ | ‑ |
| Mold temperature | 40‑80℃, recommended 50℃ | Crystallization mainly determined by mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature will cause warpage. |
| Injection pressure | 80‑140 MPa(800‑1400 bar) | Higher pressure for thin‑wall or complex‑structure parts. |
| Holding pressure | 30%‑60% of injection pressure | Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time. |
| Injection speed | Medium speed; high‑speed injection required for thin‑wall packaging containers. | ‑ |
| Screw speed | High screw speed(linear velocity 1.3 m/s) is permitted | Complete plasticization before cooling phase finishes. |
Disclaimer: All above data is for reference only.