PP Shanghai Petrochemical M700R Resin

PP Shanghai Petrochemical M700R Resin

Material Introduction: PP Shanghai Petrochemical M700R is injection‑molding grade block‑copolymer polypropylene. Featuring good impact resistance, heat resistance and chemical stability, it is widely applied in automotive, home‑appliance and other industries.

Main Applications

Automotive industry: automotive battery housings, instrument panel frames, door‑panel interior parts.

Home appliances: washing‑machine inner drums, air‑conditioner housings, fan blades, microwave‑oven supports.

Industrial products: industrial containers, pallets and turnover boxes.

Performance Parameters

Performance Category Test Item Test Condition Reference Value Unit Reference Standard Remarks & Interpretation
Basic Properties Melt Flow Rate(MFR) 230℃/2.16kg 5.2‑8.8 or 7.0±1.8 g/10 min ISO 1133 Medium‑flow block‑copolymer PP for injection molding.
Mechanical Properties Tensile Yield Strength 24.5‑31 MPa ASTM D638 Tensile yield property.
  Flexural Modulus ≥1100 MPa ASTM D790 High‑rigidity grade.
  Izod Impact Strength 23℃ ≥15(notched),>30(unnotched) J/m ASTM D256 Impact performance.
  Rockwell Hardness 84 R scale ASTM D785 Surface hardness.
Thermal Properties Heat‑Distortion Temperature(HDT) To be confirmed Data pending.
  Vicat Softening Temperature ≥150 ASTM D1525 Excellent heat‑resistance.
  Brittleness Temperature <‑32 ASTM D746 Good low‑temperature toughness.
Other Properties Yellow Index ≤4 ASTM D1925 Color‑stability indicator.
  Ash content ≤0.03 % ISO 3451‑1 Low‑ash formulation.

Injection‑Molding Process Parameters

Process Item Suggested Range / Description Remarks
Drying treatment Generally unnecessary; dry at 70‑80℃ for 2‑3 h if damp PP low‑moisture‑absorption feature.
Barrel rear zone(feed section) 160‑200℃ Prevent thermal degradation.
Barrel middle zone(compression section) 180‑220℃
Barrel front zone(metering section) 200‑240℃
Nozzle temperature 200‑240℃
Mold temperature 30‑60℃ Crystallization depends largely on mold temperature. Low temperature: poor surface, weld‑line and flow‑mark risks; high temperature brings warpage risk.
Injection pressure Adjust according to practical conditions Higher pressure for thin‑wall or complex‑structure parts.
Injection speed Adjust according to practical conditions High‑speed injection is required for thin‑wall packaging containers.
Holding pressure Adjust according to practical conditions Prevent sink mark and excessive shrinkage.

Disclaimer: All above data is for reference only.