PP Formosa Plastics 1124

PP Formosa Plastics 1124 Resin

Material Introduction: PP Formosa Plastics 1124 is well‑balanced injection‑molding homopolymer polypropylene. It features high rigidity, excellent heat resistance and good surface gloss, and complies with food‑contact safety regulations.

Main Applications

Home appliances: housings for small household electrical appliances.

Daily‑use articles: household goods, furniture, toys and stationery.

Food packaging: food containers, microwave‑safe food containers (compliant with FDA 21 CFR 177.1520).

Others: certain industrial components.

Performance Parameters

Performance Category Test Item Test Condition Reference Value Unit Reference Standard Remarks & Interpretation
Basic Properties Melt Flow Rate (MFR) 230℃/2.16kg 12‑15 g/10 min ISO 1133 High‑flow homopolymer PP for injection molding.
  Density 0.90‑0.91 g/cm³ ISO 1183 Typical homo‑PP density.
  Molding Shrinkage 1.3‑1.7 % Internal FPC Method Mold design compensation reference.
Mechanical Properties Tensile Yield Strength 34.3‑48.1 MPa ISO 527‑2 Tensile yield performance.
  Elongation at Break 50 % ISO 527‑2 Brittle‑tendency homopolymer characteristic.
  Flexural Modulus 1103‑2160 MPa ISO 178 High‑rigidity grade.
  Rockwell Hardness R‑scale 100‑115 ISO 2039‑2 Surface hardness.
  Izod Notched Impact Strength 23℃ 29‑39 J/m ISO 180 Low impact for homo‑PP.
  Izod Notched Impact Strength 23℃ 3.0 kg·cm/cm ISO 180 Unit alternative expression.
Thermal Properties Heat‑Distortion Temperature(HDT) 1.8 MPa, non‑annealed 90‑135 ISO 75‑2/A Excellent heat‑resistant performance.
  Vicat Softening Temperature 150‑157 ISO 306 Vicat softening point.
Safety Certification FDA Compliance Comply with FDA 21 CFR 177.1520 Food‑contact approval.

Injection‑Molding Process Parameters

Process Item Suggested Range / Description Remarks
Drying treatment Generally not required; dry at 80℃ for 1‑2 h if damp PP low‑moisture‑absorption characteristic.
Barrel rear zone(feed section) 160‑200℃ Avoid thermal degradation.
Barrel middle zone(compression section) 180‑220℃
Barrel front zone(metering section) 200‑240℃
Nozzle temperature 200‑240℃
Mold temperature 30‑50℃ / 40‑80℃,recommended 50℃ Crystallization depends largely on mold temperature. Low temp: poor surface, weld‑line and flow‑mark risk; High temp: warpage tendency.
Injection pressure 80‑140 MPa(800‑1400 bar), max 1500‑1800 bar Raise pressure for thin‑wall or complex parts.
Holding pressure 30%‑60% or 80% of injection pressure Prevent sink mark and excessive shrinkage; holding time accounts for ~30% of cycle time.
Injection speed High‑speed injection minimizes internal pressure; adopt low‑speed under higher melt temperature for surface defects.
Screw speed Permitted high screw speed (linear velocity 1.3 m/s) Complete plasticization before cooling phase ends.
Runner & gate Runner diameter:4‑7 mm. Pin‑point gate:length 1‑1.5 mm, min diameter 0.7 mm. Edge gate:short length (~0.7 mm), depth=1/2 wall‑thickness, width=2×wall‑thickness.
Mold venting: vent depth 0.025‑0.038 mm, width 1.5 mm for good exhaust.

Disclaimer: All above data is for reference only。