PP‑R Daqing PPB4228

Daqing Refining & Chemical PPB4228 Resin

Material Introduction: Daqing Refining & Chemical PPB4228 is impact‑modified random‑copolymer polypropylene (PP‑R). It delivers balanced low‑temperature toughness and rigidity. Benefiting from excellent impact resistance and heat resistance, combined with block‑copolymer PP (PPB) characteristics, it exhibits favorable pressure‑bearing performance for pipe applications.

Main Applications

Suitable for extrusion of pipes and profiles, widely used in building materials industry, especially for cold‑hot‑water pipes and heating pipes.

Performance Parameters

Performance Category Test Item Test Condition Typical Value Unit Remarks & Interpretation
Physical Properties Melt Flow Rate (MFR) 230℃, 2.16 kg 0.37 g/10 min Low‑flow grade for pipe extrusion.
Mechanical Properties Tensile Yield Stress ≥23.2 MPa Tensile yield performance.
  Flexural Modulus ≥921 MPa Stiffness index.
  Izod Notched Impact Strength -20℃ 6.6 kJ/m² Low‑temperature impact resistance.

Pipe Extrusion Process Parameters

Process Item Typical Reference Range Remarks
Drying temperature / time 80‑90℃ / 2‑3 h Low moisture absorption for PP; drying stabilizes pipe appearance and performance.
Extruder barrel zone 1(feed section) 180‑190℃
Extruder barrel zone 2(compression section) 190‑210℃
Extruder barrel zone 3(metering section) 210‑220℃
Head & die temperature 210‑230℃ Ensure homogeneous melt flow and reduce internal stress.
Screw speed Adjust by pipe diameter & output Match with haul‑off speed for stable dimension.
Haul‑off speed Constant, synchronized with extrusion speed
Sizing method Vacuum sizing & water cooling Guarantee pipe roundness and smooth inner / outer surface.

Disclaimer: All above data is for reference only.