PP‑R Yangzi Petrochemical PPR‑M00(YPR‑503 / R503)

PP‑R Yangzi Petrochemical PPR‑M00(YPR‑503 / R503)Resin

Material Introduction: PP‑R Yangzi Petrochemical PPR‑M00 (alias YPR‑503 / R503) is random‑copolymer polypropylene pipe‑special resin. It features high impact resistance, excellent heat‑aging resistance and favorable long‑term hydrostatic strength, especially suitable for high‑demand cold‑hot‑water transmission systems.

Main Applications

Building cold‑hot‑water transmission systems: domestic cold‑hot‑water pipelines, central heating systems.

Drinkable purified‑water supply system: qualified sanitary performance for potable‑water piping.

Floor heating system: manufacturing floor‑heating pipes.

Central air‑conditioning system: refrigerant‑water pipelines for air‑conditioning.

Chemical piping system: conveyance or discharge of certain chemical media.

High‑performance multi‑layer composite pipes: base material for antibacterial pipe, UV‑resistant pipe, high‑light‑shielding pipe and other multi‑layer composite pipes.

Performance Parameters

Performance Category Test Item Test Condition Test Standard Typical Value Unit Remarks & Interpretation
Basic Properties Melt Flow Rate (MFR) 230℃/2.16kg GB/T 3682 0.27‑0.30 g/10min Low‑flow grade for pipe extrusion.
Mechanical Properties Tensile Yield Strength GB/T 1040 22.9‑23 MPa Tensile yield property.
  Elongation at Break GB/T 1040 500 % Good ductility and toughness.
  Flexural Modulus GB/T 9341 629‑800 MPa Material rigidity index.
  Charpy Notched Impact Strength 23℃ GB/T 1043.1 61 kJ/m² Room‑temperature notch impact performance.
  Charpy Notched Impact Strength -20℃ GB/T 1043.1 2.8 kJ/m² Low‑temperature notch impact performance.
  Izod Notched Impact Strength 23℃ GB/T 1843 25 kJ/m² Cantilever‑beam impact resistance.
Thermal Properties Heat‑Distortion Temperature GB/T 1634.2 65 Thermal deformation reference.
  Oxidation Induction Time(OIT) GB/T 19466.6 80.1 min Excellent thermal‑oxidative aging resistance for long‑term pipe service.

Pipe Extrusion Process Parameters

  • Barrel temperature: 185205℃; adapter block 200205℃; die head 200~205℃.

Typical parameters for three‑layer co‑extrusion composite pipe:

  • Inner layer: Zone1 190℃, Zone2 200℃, Zone3 200℃, Zone4 205℃, Die 205℃
  • Middle layer: Zone1 195℃, Zone2 200℃, Zone3 200℃, Zone4 200℃, Adapter 200‑205℃, Die 205℃
  • Outer layer: Zone1 185℃, Zone2 195℃, Zone3 200℃, Zone4 200℃, Die 200℃
  • Main extruder speed: adjust according to pipe diameter & wall thickness, typical 25‑40 rpm.
  • Screw torque: typical range 45%‑65%.

Injection‑Molding Process Parameters

  • Barrel temperature:180280℃,typical melt temperature 220280℃。
  • Mold temperature:20‑70℃. Higher mold temperature improves surface gloss and dimensional stability.
  • Injection pressure:80‑140 MPa(800‑1400 bar); up to 180 MPa for thin‑wall articles.
  • Holding pressure:30%‑60% of injection pressure.
  • Injection speed:medium‑high speed recommended.