LLDPE Daqing Petrochemical DNDA‑8320 Resin

Material Introduction: LLDPE Daqing Petrochemical DNDA‑8320 is high‑flow linear low‑density polyethylene. It is mainly applied for injection‑molding process to produce various daily‑use articles and containers.

Main Applications

Household utensils: waste bins, storage boxes, containers, lids.

Daily‑use articles: toys, refrigerator accessory components.

Other applications: garbage‑bag films, bottle‑cap raw material, coating‑grade PE according to reference documents.

Performance Parameters

Performance Category Test Item Test Method / Condition Test Data / Unit Remarks & Interpretation
Basic Properties Density GB/T 1033.2 0.924‑0.926 g/cm³ Typical LLDPE density range.
  Melt Flow Rate (MFR) GB/T 3682 (190°C/2.16kg) 20 g/10min High‑flow feature adapts to injection molding, realizes fast cavity filling for thin‑wall articles.
Mechanical Properties Tensile Yield Stress GB/T 1040.2 ≥10 MPa Indicator of tensile‑deformation resistance.
  Tensile Stress at Break GB/T 1040.2 ≥4 MPa Maximum stress the material can withstand before fracture.
  Elongation at Break GB/T 1040.2 ≥100%‑600% Good toughness and ductility for large‑deformation condition; data range from different sources.
  Charpy Notched Impact Strength (23℃) GB/T 1043.1 54‑69 kJ/m² Good room‑temperature impact resistance; data from different sources.
Appearance Property Pellet Appearance (Discolored Pellets) SH/T 1541 ≤5 pcs/kg (premium grade) Purity indicator; lower value means fewer impurities.
  Black Pellets SH/T 1541 0 pcs/kg Same as above.
Other Features Additive Non‑added Neat resin, favorable base for subsequent modification such as color‑matching.

Injection‑Molding Process Parameters

Process Parameters Recommended Range Remarks & Interpretation
Drying Treatment Normally not required Low‑hygroscopic LLDPE. Drying is unnecessary under good storage. Dry at 60‑70 °C for 1‑2 h as precaution if package damaged or high‑humidity environment.
Barrel Temperature 160‑220 °C Temperature rises from rear zone to front zone. Reference setting: rear 160‑180°C, middle 180‑200°C, front 190‑220°C. Start debugging at medium‑low temperature to avoid thermal degradation for this high‑MFR grade.
Mold Temperature 30‑60 °C Low mold temperature (30‑40°C) shortens cycle time and prevents deformation; higher mold temperature improves surface gloss and reduces internal stress.
Injection Pressure Medium pressure High flowability permits medium‑low injection pressure. Excessive pressure causes flash; adjust according to product structure and dimension.
Injection Speed Medium‑high speed Fast injection takes advantage of high flowability, improves productivity, especially for thin‑wall parts.
Holding Pressure 40%‑60% of injection pressure Avoid excessive holding pressure and long holding time to reduce internal stress.
Back Pressure 0.5‑1.5 MPa Low back pressure for melt compaction; excessive back pressure generates redundant shear heat.
Screw Speed 50‑100 rpm Moderate rotating speed, prevent excessive shear heat accumulation.

Disclaimer: All above data is for reference only.