LLDPE SABIC 218WJ

LLDPE SABIC 218WJ Resin

Material Introduction: LLDPE SABIC 218WJ is a high‑performance linear low‑density polyethylene. It features easy processability, good tensile properties, impact strength and optical performance, mainly applied for blown‑film products.

Main Applications

Various packaging bags: shopping bags, garbage bags, inner liner bags.

Laminated & co‑extruded films: laminated films, co‑extruded films and consumer‑goods packaging.

Other film products: thin liners.

Performance Parameters

Performance Category Test Item Test Method / Condition Value & Unit Remarks & Interpretation
Basic Properties Density ASTM D‑1505 / D‑792 0.918 g/cm³ Typical density range for LLDPE.
  Melt Flow Rate (MFR) ASTM D‑1238 (190°C/2.16 kg) 2.0 g/10min Good melt flowability, suitable for film processing.
Mechanical Properties Elongation at Break (MD) ASTM D‑882 700 % Excellent machine‑direction ductility of film.
  Elongation at Break (TD) ASTM D‑882 750 % Excellent transverse‑direction ductility of film.
  1% Secant Modulus (MD) ASTM D‑882 220 MPa Machine‑direction rigidity of film.
  1% Secant Modulus (TD) ASTM D‑882 260 MPa Transverse‑direction rigidity of film.
  Dart Drop Impact Strength ASTM D‑1709 85‑110 g Puncture‑resistance and impact‑resistance; higher value represents better performance; slight deviation among sources.
  Elmendorf Tear Strength (MD) ASTM D‑1922 130‑135 g Machine‑direction tear resistance.
  Elmendorf Tear Strength (TD) ASTM D‑1922 320‑400 g Transverse‑direction tear resistance, much higher than MD direction; slight deviation among sources.
  Tensile Strength at Break (MD) ASTM D‑882 35 MPa Machine‑direction tensile capacity of film.
  Tensile Strength at Break (TD) ASTM D‑882 29‑59 MPa Transverse‑direction tensile capacity of film; slight deviation among sources.
Optical Properties Haze ASTM D‑1003 13‑15 % Transparency indicator; lower value means higher transparency.
  Gloss (60°) ASTM D‑2457 60‑80 Surface‑gloss indicator; slight deviation among sources.
Thermal Properties Vicat Softening Temperature ASTM D‑1525 98 °C Heat‑resistance indicator.
Additives Slip Agent approx. 1500 ppm Improve surface slip property for processing and end‑use.
  Anti‑blocking Agent approx. 3500 ppm Prevent blocking between film layers.

Blown‑Film Processing

For mainstream blown‑film extrusion, temperature, pressure and other parameters shall be optimized according to equipment, film thickness and performance requirements. General processing temperature range for LLDPE blown‑film: 150‑210 ℃.

Blown‑Film Processing Notes

Shear sensitivity: LLDPE presents low shear sensitivity and maintains higher viscosity under shearing such as extrusion, which makes it harder to process than LDPE with identical MFR. ‑ Equipment requirements: Extruders for LLDPE may require higher driving power, higher melt temperature and pressure. Die gap shall be widened (e.g. from LDPE 0.024‑0.040 inch to 0.060‑0.10 inch) to avoid excessive back‑pressure and melt fracture. ‑ Bubble stability: LLDPE blown‑film bubble stability is inferior to LDPE. Dual‑lip air ring is recommended to improve cooling and bubble stability. ‑ Blending for better processability: Many film producers blend LLDPE with LDPE (e.g. 50 % each) to optimize processability and raise output capacity。