PC LG Chem 1303AH‑15
PC LG Chem 1303AH‑15
Material Introduction: PC LG Chem 1303AH‑15 is a 15 % glass‑fiber‑reinforced polycarbonate resin. It combines the excellent properties of PC with mechanical strength and dimensional stability brought by glass‑fiber reinforcement. It is suitable for engineering components requiring high strength, flame‑retardant performance, electrical insulation, heat resistance and dimensional accuracy.
Main Applications
‑ Electronic & Electrical: Circuit‑breaker housings, charger shells, relay bases, 5G‑equipment brackets. ‑ Automotive Parts: Sensor brackets, connectors, lamp holders, interior fasteners. ‑ Industrial Parts: Gears, pump housings, instrument frames. ‑ Household Equipment: Power‑tool housings, vacuum‑cleaner air ducts, high‑temperature kettle components.
Physical Properties
| Performance Category | Test Standard | Unit | Typical Value |
|---|---|---|---|
| Physical Properties | |||
| Density | ISO 1183 | g/cm³ | 1.34 |
| Water Absorption (24 h) | ISO 62 | % | 0.12 |
| Mechanical Properties | |||
| Tensile Strength | ISO 527‑2 | MPa | 110‑125 |
| Flexural Modulus | ISO 178 | MPa | 5500‑6500 |
| Izod Notched Impact Strength | ISO 180/1A | kJ/m² | 8‑10 |
| Thermal Properties | |||
| Melting Temperature (Tm) | ISO 11357 | °C | 225‑230 |
| HDT (1.82 MPa) | ISO 75 | °C | 135‑140 |
| Vicat Softening Point | ISO 306 | °C | 148 |
| Electrical Properties | |||
| Volume Resistivity | IEC 60093 | Ω·cm | >10¹⁵ |
| Dielectric Strength | IEC 60243 | kV/mm | 30 |
| CTI (Comparative Tracking Index) | IEC 60112 | V | 250‑275 |
| Flame‑Retardant Property | UL94 | ‑ | V‑0 (0.8 mm) |
Injection Molding Parameters
| Process Parameter | Unit | Recommended Range | Key Notes |
|---|---|---|---|
| Drying Condition | ‑ | ‑ | Strict drying is mandatory! |
| Drying Temperature | °C | 100‑120 | Avoid high‑temperature caking |
| Drying Time | h | ≥4 | Moisture content shall be <0.02 % |
| Barrel Temperature | ‑ | ‑ | Segmented control to prevent thermal degradation |
| Rear Section (Feed Zone) | °C | 260‑280 | Too low temperature causes poor glass‑fiber dispersion |
| Middle Section (Plasticizing Zone) | °C | 280‑300 | |
| Front Section (Nozzle) | °C | 290‑310 | Avoid excessive residence time |
| Mold Temperature | °C | 80‑100 | Affects surface gloss and internal stress |
| Injection Pressure | MPa | 70‑120 | Medium‑to‑high pressure required for high glass‑fiber content |
| Holding Pressure | % | 50‑70 % of injection pressure | Reduce sink marks; excessive pressure causes flash |
| Screw Speed | rpm | 40‑80 | Low speed to prevent excessive shear fracture of glass fibers |
| Back Pressure | MPa | 0.3‑0.7 | Stabilize plasticizing; prevent air entrapment |
Disclaimer: All above data is for reference only.