PC Lihuayi Weiyuan WY‑111BR

PC Lihuayi Weiyuan WY‑111BR

Material Introduction: PC Lihuayi Weiyuan WY‑111BR is a medium‑viscosity, injection‑molding grade polycarbonate material. It is adopted for favorable mechanical performance, high transparency and flame‑retardant properties. Its core advantages include high strength, high rigidity, excellent impact resistance and good heat resistance.

Main Applications

  1. Electronic & Electrical Components: Electrical accessories, telephone housings, telephone exchangers, signal relays, capacitors and other communication‑equipment & office‑device parts.
  2. Automotive Industry: Automotive components, lamp housings, etc.
  3. Consumer Goods & General‑Purpose Parts: Daily‑use articles.
  4. Industrial Equipment & Components: Industrial mechanical parts.
  5. Optical Lighting: Large‑size lamp housings, protective glazings benefited from high transparency.

Key Characteristics

Characteristic Category Description Reference Data (Test Standard)
Physical Properties Medium‑viscosity, slight‑blue transparent, easy‑to‑release Density: 1.20 g/cm³ (ASTM D792)
MFR: 11 g/10min (300°C/1.2kg, ASTM D1238)
Mechanical Properties High rigidity, high strength, excellent impact resistance Tensile Yield Strength: 59 MPa (ASTM D638) or >60 MPa (ISO 527)
Elongation at Break: 88% (ASTM D638 / ISO 527)
Flexural Modulus: 2350‑2400 MPa (ASTM D790) or 3100 kg/cm² (≈304 MPa)
Flexural Strength: 90.2 MPa (ASTM D790) or 103 kg/cm² (≈10.1 MPa)
Charpy Notched Impact Strength (23°C): 71 kJ/m² (ISO 179) or 85.3 kg·cm/cm
Thermal Properties Good heat resistance Vicat Softening Temperature: 148°C (Rate B; ASTM D1525) or 153.2°C
HDT (1.8 MPa): ~125°C (Inferred from similar PC grades)
Optical Properties High transparency Light Transmittance: 89.0% or 90.1% (ASTM D1003 / ISO 13468)
Haze: <0.80% or 0.36% (ISO 14782)
Safety Properties Flame retardancy UL94: V‑2 (1.5 mm or 1.6 mm)
Processing Properties Injection‑molding grade; sufficient pre‑drying required to prevent hydrolytic degradation Recommended moisture content <0.02%

Injection Molding Processing Parameters

Processing Stage Parameter Item Suggested Range / Operation Notes Unit / Remarks
Pre‑drying Drying Temperature 110‑120 °C
  Drying Time 8‑10 (or more than 4 hours) h (dehumidifying dryer recommended)
  Allowable Moisture Content < 0.02% Critical requirement
Injection Temperature Rear Barrel Temperature 210‑240 °C
  Middle Barrel Temperature 230‑280 °C
  Front Barrel Temperature 240‑285 °C
  Nozzle Temperature 240‑250 °C
  Melt Temperature 260‑290 (reference range, confirm by air‑shot test) °C (shall not exceed 310 °C to avoid degradation)
  Mold Temperature 50‑100 (commonly 80‑100) °C (higher mold temperature reduces internal stress, improves filling and surface appearance)
Injection Settings Injection Pressure 80‑130 MPa
  Holding Pressure MPa (normally 40%‑60% of injection pressure)
  Back Pressure ~10 bar (≈1 MPa) MPa/bar (can be reduced without silver streaks or color‑mixing defects)
  Screw Speed 28‑70 rpm
Time Settings Injection Time 20‑90 s
  High‑Pressure Holding Time 0‑5 s
  Cooling Time 20‑90 s
  Total Cycle Time 40‑190 s

Disclaimer: All above data is for reference only.