PMMA Sumitomo Chemical MH

PMMA Sumitomo Chemical MH

PMMA Sumitomo Chemical MH is general‑purpose polymethyl methacrylate with good heat‑resistance and outstanding optical performance. It also features favorable mechanical properties, excellent electrical insulation and dimensional stability.

Main Applications

Automotive industry: indicator lamp & taillight housings, instrument housings, rear decorative panels, instrument display screens.

Optics & lighting: sunglass lenses, optical lenses, lamp covers, diffusion panels.

Electrical & electronics: transparent insulating components.

Sheets & profiles: extruded sheets, tubes and rods for construction and decoration.

Industrial applications: components requiring high transparency and moderate heat‑resistance.

Properties

Property Category Item Test Standard Value Unit
Physical Density JIS K7112 1.19 g/cm³
  Water absorption (24 h) JIS K7209 0.3 %
  MFR(230℃/3.8 kg) JIS K7210 2.0 g/10min
  Molding shrinkage (flow direction) ASTM D955 0.20‑0.60 %
  Refractive index JIS K7105 1.49
  Light transmittance (3.2 mm) JIS K7105 93.0 %
  Haze JIS K7105 <0.5 %
Mechanical Tensile strength (yield) JIS K7113 76.0 MPa
  Flexural strength JIS K7203 120 MPa
  Flexural modulus JIS K7203 3200 MPa
  Elongation at break JIS K7113 13 %
  Rockwell hardness‑M JIS K7202 M100
  Charpy notched impact JIS K7110 1.4 kJ/m²
Thermal HDT (1.8 MPa, annealed) JIS K7207 101
  Vicat softening temperature JIS K7206 109
  Linear thermal expansion coefficient ASTM D696 7.0×10⁻⁵ cm/cm/℃
Electrical Volume resistivity JIS K6911 >1.0×10¹⁵ Ω·cm
  Surface resistivity JIS K6911 >1.0×10¹⁶ Ω
  Dielectric constant (60 Hz) JIS K6911 3.10
  Dissipation factor (60 Hz) JIS K6911 0.04
Flammability UL94 (1.5 mm) UL94 HB class

Injection‑Molding Parameters

Process Item Recommendation Notes
Predrying Drying temperature 80‑85 ℃ / 91 ℃ Desiccant dryer required
  Drying time 4‑5 h / 2‑4 h Target moisture<0.1%, eliminate bubbles & silver‑streaks
Barrel setting Rear zone 185‑205 ℃ Melt onset ~160 ℃, decomposition>270 ℃
  Middle zone 220‑240 ℃  
  Front zone 210‑230 ℃  
  Nozzle 210‑230 ℃  
  Melt temperature 238‑272 ℃ Strictly control residence time to avoid degradation
  Mold temperature 34‑71 ℃ Higher temp improves gloss yet lengthens cycle time
  Injection pressure 80‑140 MPa High‑viscosity material; easy to generate internal stress with fast cooling
  Injection speed Medium Excessive speed causes surface defects & internal stress

Note: All data for reference only, please refer to official TDS for mass‑production.