PBT CHANG CHUN 4830‑BK

PBT CHANG CHUN 4830‑BK

PBT CHANG CHUN 4830‑BK is a 30 % glass‑fiber‑reinforced PBT resin with UL94 V‑0 flame‑retardant rating. Glass‑fiber reinforcement greatly improves mechanical strength, rigidity, heat resistance and dimensional stability.

Main Applications

Electrical & Electronics (core application): connectors, switch components, sockets, coil bobbins, rectifiers, TV parts, cooling fans.

Automotive industry: motorcycle & automotive components.

Household appliances: home‑appliance parts.

Industrial parts: power‑tool accessories.

Physical‑Mechanical‑Thermal‑Electrical Properties

Property Category Property Item Test Standard Test Data / Range Unit
Physical Properties Density ASTM D792 1.56‑1.64 g/cm³
  Glass‑fiber content Ash / CCP 30 %
  Water absorption ASTM D570 0.03 %
  Molding shrinkage ASTM D955 0.2‑1.4 %
Mechanical Properties Tensile strength ASTM D638 1100‑1400 kg/cm²
  Tensile strength (converted) ~117.6 MPa
  Elongation at break ASTM D638 2.5‑4.5 (or 4‑5) %
  Flexural strength ASTM D790 1500‑2300 kg/cm²
  Flexural strength (converted) ~186.2 MPa
  Flexural modulus ASTM D790 70000‑100000 kg/cm²
  Flexural modulus (converted) ~6860 MPa
  Izod notched impact ASTM D256 7‑11 (or 7.0‑13.0) kg·cm/cm
  Rockwell hardness ASTM D785 M94 / R121
Thermal Properties HDT @1.8 MPa ASTM D648 200‑208
  HDT @0.45 MPa ASTM D648 218‑220
  Melting point DSC 225
  CLTE ASTM D696 3×10⁻⁵ cm/cm/℃
  UL94 rating UL94 V‑0 (1.6 mm / 3.0 mm) class
Electrical Properties Volume resistivity ASTM D257 >10¹⁵ Ω·cm
  Surface resistivity ASTM D257 >10¹³‑>10¹⁴ Ω
  Dielectric strength ASTM D149 >20‑23 kV/mm
  Arc resistance ASTM D495 90‑100 sec
  Relative permittivity (60 Hz) ASTM D150 3.0‑3.5
  Dissipation factor (60 Hz) ASTM D150 0.001

Injection‑Molding Parameters

Process Stage Parameter Item Reference Range / Recommendation Unit / Remarks
Pre‑treatment Drying temperature 120‑150
  Drying time 6‑8 h@120 ℃ or 2‑4 h@150 ℃(bed thickness<30 mm) h
  Target moisture content <0.02‑0.03 %
  Drying equipment Desiccant dryer recommended
Injection Molding Barrel temperature 235‑260; keep lower for FR grade to avoid degradation
  Nozzle temperature 5‑10 ℃ lower than front barrel zone
  Melt temperature 240‑260
  Mold temperature 40‑100; commonly 70‑90 ℃; 65 ℃ for FR‑GF grade
  Injection pressure 40‑100 MPa
  Injection speed High speed; prevent surface freezing due to fast PBT crystallization
  Back pressure Set according to melt condition, generally low MPa
  Screw speed Adjust by equipment & cycle; avoid excessive shear heat rpm
Post‑processing Annealing temperature (if required) 120‑150; reduce residual stress & improve dimensional stability
  Annealing time 1‑2 h
Regrind material Reuse ratio <25 %; material must be clean & non‑degraded %

Note: All data above is for reference only.