TPU Covestro 1209

TPU Covestro 1209

TPU Covestro 1209 is thermoplastic polyurethane elastomer, available in polyester‑based and polyether‑based versions. It features broad hardness range (60HA‑85HD), good abrasion‑resistance, oil‑resistance, transparency and elasticity, coupled with high tensile strength and tear resistance.

Main Applications

Footwear: shoe soles, insoles, buffer components. Industrial parts: seals, gaskets, rollers, transmission belts. Tubes & profiles: hoses, conduits, cable jackets. Automotive parts: dust‑boots, vent blades and other consumer goods.

Physical Properties

Property Category Item Test Condition Test Standard Typical Reference Data Unit
Physical Properties Specific gravity / Density ASTM D792 1.07 g/cm³
Mechanical Properties Shore Hardness ASTM D2240 70 Shore A
  Tensile Strength ASTM D412 25.5 MPa
  Elongation at Break ASTM D412 770 %
  Flexural Modulus 23℃ ASTM D790 18.6 MPa
  Tear Strength ASTM D624 60.5 kN/m
Thermal Properties Glass Transition Temperature ‑57
  Vicat Softening Temperature ASTM D1525 75
Other Properties Compression Set 22 h ASTM D395B 30 %
  Abrasion Loss ASTM D3489 7 mg
  Molding Shrinkage (flow direction) ASTM D955 0.008 mm/mm

Processing Parameters

Process Parameter Unit Reference Range Remarks
Pre‑drying Drying temperature 80‑110 Circulating hot‑air drying recommended; TPU is moisture‑sensitive, drying is mandatory
  Drying time h ≥3 Until moisture<0.05%
  Material bed thickness mm ≤30 Guarantee drying efficiency
Injection molding Rear feed zone temp 150‑175 Reference for 85A‑98A grades; avoid premature plasticization
  Middle compression zone temp 160‑185 Adjust according to formulation & equipment
  Front metering zone temp 170‑195 Adjust according to formulation & equipment
  Nozzle temperature Equal‑to‑slightly lower than front zone Prevent drooling or cold‑plug blockage
  Melt temperature 170‑195 Strictly prohibit>240℃ to avoid degradation; avoid long‑term melt residence
  Mold temperature 25‑45  
  Injection pressure bar 50‑100 Keep as low as possible while full filling
  Hold‑pressure bar 30%‑60% of injection pressure Excessive hold‑pressure & long hold‑time shall be avoided to reduce internal stress
  Screw speed rpm 50‑100 High speed causes shear overheating
  Back pressure bar 5‑15 Improve melt homogeneity; excessive back‑pressure generates extra heat

Note: All information above is for reference only!

 