PC/ABS SABIC C1100HF

PC/ABS SABIC C1100HF

PC/ABS SABIC C1100HF is a high‑flow alloy material. It combines the mechanical strength, heat resistance and UV‑resistance of polycarbonate (PC), as well as excellent processing flowability of ABS.

Main Applications

Automotive Parts: automotive interior and exterior components such as wheel‑housings, mirror housings.

Electrical‑Electronic: housings and internal parts for notebooks, desktops, copiers, printers and other business equipment; electrical appliances, lawn‑and‑garden machinery.

Telecommunications: mobile‑phone housings & accessories, smart cards (SIM‑cards).

Home Appliances: internal and external parts for washing machines, hair dryers, microwave ovens.

Physical Properties

Property Category Test Item Test Standard Data Unit
Physical Properties Density / Specific Gravity ASTM D792 1.15 g/cm³
  Melt Flow Rate (MFR) 260°C/5.0 kg, ASTM D1238 19 g/10 min
  Mold Shrinkage (Flow, 3.20 mm) Internal Method 0.50‑0.70 %
  Water Absorption (24hr) ASTM D570 0.10 %
Mechanical Properties Tensile Modulus ASTM D638 2280 MPa
  Tensile Strength (Yield) ASTM D638 57.2 MPa
  Elongation at Break ASTM D638 150 %
  Flexural Modulus ASTM D790 2340 MPa
  Flexural Stress (Yield) ASTM D790 88.3 MPa
  Izod Notched Impact Strength (23°C) ASTM D256 590 J/m
  Izod Notched Impact Strength (-30°C) ASTM D256 480 J/m
Thermal Properties Heat‑Distortion Temperature (1.8 MPa, unannealed, 3.20 mm) ASTM D648 113 °C
  Heat‑Distortion Temperature (0.45 MPa, unannealed, 3.20 mm) ASTM D648 129 °C
  Vicat Softening Temperature ISO 306 130 °C
  Relative Temperature Index (RTI Elec) UL 746 105 °C
Flame Retardancy UL 94 Rating (1.19 mm) UL 94 HB

Processing Parameters

Process Parameter Unit Recommended Value / Range
Drying Treatment    
Drying Temperature °C 100‑110
Drying Time h 3.0‑4.0
Recommended Moisture Content % 0.020
Injection Molding Temperature    
Rear Barrel Temperature °C 250‑290
Middle Barrel Temperature °C 255‑295
Front Barrel Temperature °C 260‑300
Nozzle Temperature °C 275‑300
Melt Temperature °C 275‑300
Mold Temperature °C 60.0‑90.0
Screw Parameters    
Back Pressure MPa 0.300‑0.700
Screw Speed rpm 40‑70
Vent Depth mm 0.038‑0.076
Injection Parameters    
Suggested Shot Volume % 30‑80

Note: All information above is for reference only!